Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 7RE10 is an austenitic, stainless chromium-nickel steel of the 25/20 type. It has good resistance to carburization, sulfidation and oxidation combined with moderate creep strength and structural stability. Maximum service temperature in air is 1100°C (2010°F).

Standards

  • ASTM: 310S, 310H
  • UNS: S31008, S31009
  • EN Number: 1.4845
  • W.Nr.: 1.4845
  • DIN: X12 CrNi 25 21
  • SS: 2361
  • AFNOR: Z12CN25-20
  • BS: 310S31

Product standards

ASTM A-314
Suitable for production of flanges etc. acc. to ASTM A-182

Certificates

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.