Sandvik 8LR30

BilletsDatasheet

Datasheet updated 2019-11-14 13:31 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 8LR30 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service but also has good mechanical strength at high temperatures.

Standards

  • ASTM: 321/321H
  • UNS: S32100
  • EN Number: 1.4541
  • W.Nr.: 1.4541
  • SS: 2337
  • BS: 321S31

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for production of flanges etc. acc. to ASTM A-182

Certificates

Status according to EN 10 204 3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.