Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanmac® 304/304L is an austenitic chromium-nickel steel with improved machinability.

Standards

  • ASTM: 304, 304L
  • UNS: S30400, S30403
  • EN Number: 1.4301, 1.4307
  • EN Name: X 5 CrNi 18-10, X 2 CrNi 18-9
  • W.Nr.: 1.4301

Product standards

  • EN 10088-3
  • ASTM A-314

Suitable for the production of flanges etc. according to ASTM A-182 grade F304/304L.

Certificates

Status according to EN 10 204/3.1

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.