Poly a fast running, general purpose, Class 155 polyurethane wire enamel. Suitable for monolithic or dual coat applications, it meets the requirements of NEMA MW 75, MW 80 (MW 79 on finer gauges) also meets the requirements of JIS C 3003 for 'Pinhole' resistance.
Poly is available in clear and colored versions.
The primary benefit of the polyurethane is its easy solderability vs. the 180C tri-2-SOd solderable Polyester coating ( 2 seconds at 380°C vs. 5 seconds at 455°C)
Polyurethane can be readily used on Copper, Aluminium and Copper-Clad Aluminium wires as a basecoat for the commonly applied thermoplastic bond coats. It is a cost-effective insulation to be applied to wires that are used in the manufacture of precision coils, as it provides end users manufacturing benefits in handling and solderability.
Typical applications are within motors, R.F. coils, relay, encapsulated coils, ignition coils, solenoids, low voltage transformers, Multi layer and precision wound coils, speaker voice coils.
Electrical properties
Property | NEMA MW-1000 | ASTM D1676 | IEC 851 | JIS C 3003 | (AWG 24) |
---|---|---|---|---|---|
Dissipation factor at 170°C (338°F) - 1 kHz | 0.22 |
Mechanical properties
Property | NEMA MW-1000 | ASTM D1676 | IEC 851 | JIS C 3003 | (AWG 24) |
---|---|---|---|---|---|
Adherence and flexibility | Pass 1d | Pass 1d | |||
Cut-through temperature | 223°C (433°F) | ||||
Heat shock 20% stretch - ½ h at 175°C (347°F) |
Pass 3d |
Soldering properties
Property | NEMA MW-1000 | ASTM D1676 | IEC 851 | JIS C 3003 | (AWG 24) |
---|---|---|---|---|---|
at 340°C (644°F) - without/ with flux |
10.0/7.0 sec |
10.0/7.0 sec |
10.0/7.0 sec | 10.0/7.0 sec | 10.0/7.0 sec |
at 360°C (680°F) - without/ with flux | 4.0/3.0 sec | 4.0/3.0 sec | 4.0/3.0 sec | 4.0/3.0 sec | 4.0/3.0 sec |
at 380°C (716°F) - without/ with flux | 2.0/1.5 sec | 2.0/1.5 sec | 2.0/1.5 sec | 2.0/1.5 sec | 2.0/1.5 sec |