Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

PolyClad a magnet wire THEIC modified Polyester insulation. It has excellent thermal endurance and solvent resistance.

Typical applications are within appliance and tool motors, continuous operation coils, subfractional instrument and servo motors solenoids, transformers, speaker voice coils.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.