Sandvik 14C28N®

Strip steelDatasheet

Datasheet updated 2020-08-27 12:17 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 14C28N® is a martensitic stainless chromium steel with a chemistry optimized for high quality professional knife applications. The chemical composition provides a unique combination of properties including:

  • Excellent edge performance
  • Very high hardness
  • Good corrosion resistance

Sandvik 14C28N® is mainly recommended for knife applications which put very high demands on edge sharpness, edge stability and corrosion resistance. Examples are pocket knives, chefs knives, hunting knives and fishing knives.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email