Sandvik 20C

Strip steelDatasheet

Datasheet updated 2019-10-03 08:20 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 20C is a hardened and tempered carbon steel characterized by good properties in respect of:

  • Fatigue strength and wear resistance
  • Hardness combined with ductility
  • Dimensional tolerances
  • Surface and edge finishes
  • Shape

The material also has good blanking and forming properties, retaining the shape of the parts after the blanking operation.

Standards

  • ASTM: 1095
  • EN Number: 1.1274

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.