Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 10C28Mo2 is a martensitic stainless chromium steel developed for razor blade and knife applications with high demands on corrosion resistance. The carefully chosen chemical composition in combination with a very fine microstructure also provides a high hardness, good edge retention, toughness and edges that are easy to re-sharpen.

After heat treatment the grade is characterized by:

  • Very good corrosion resistance
  • High hardness which gives good wear resistance
  • Good toughness

Typical applications for Sandvik 10C28Mo2 are kitchen knives and other tools where a dishwasher-safe material is required, professional butcher knives that need to be easily re-sharpened, outdoor knives, medical blades and razor blades, with high requirements on corrosion resistance and toughness.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.