Sandvik 12R11

Strip steelDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 12R11 is an austenitic stainless, general purpose steel with good spring properties that in most cases fulfill demands regarding corrosion resistance, mechanical strength, fatigue and relaxation properties.

Service temperature: up to 250°C (480°F)

Standards

  • ASTM: (301)
  • EN Number: 1.4310
  • EN Name: X 10 CrNi 18-8
  • SS: 2331

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email