Sandvik 13RM19

Strip steelDatasheet

Datasheet updated 2020-08-27 14:05 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 13RM19 is a stainless spring steel combining high mechanical strength with a non-magnetic structure. This combination of properties has previously been found mainly in expensive Co-Ni-base or Cu-Be alloys. Corrosion resistance is comparable to ASTM 301.

Sandvik 13RM19 also possesses good fatigue properties and excellent ductility, which makes it a most suitable choice for springs and other high-strength applications where ferromagnetic materials cannot be used.

Sandvik 13RM19 main characteristics:

  • Non-magnetic structure in all conditions
  • High mechanical strength in the cold rolled condition. Strength can be further increased by tempering, without any effect on the non-magnetic structure.
  • High elastic limit and energy storing capacity in the cold rolled and tempered condition which is important for spring applications.

Service temperature: up to 250°C (480°F)

Standards

  • EN Number: 1.4369
  • EN Name: X 11 CrNiMnN 19-8-6

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.