Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 15R10 is an austenitic chromium-nickel (CrNi) stainless steel used as a base material for Sandvik coated strip steel. The product is particularly suited to many types of electric load carrying spring applications, such as contact springs and tactile domes.

Sandvik 15R10 is characterized by good corrosion resistance, mechanical strength and excellent fatigue and relaxation properties, as well as superior contact properties and/or solderability, achieved through the right choice of coating layer.

Standards

  • ASTM: (301)
  • EN Number: 1.4310
  • EN Name: X 10 CrNi 18-8

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.