Sandvik 2RK65™ HV

Strip steelDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 2RK65™ HV is a vacuum arc-remelted high-alloy austenitic stainless steel with very high cleanliness resulting in good polishability. The grade is also characterized by very good overall corrosion resistance and good weldability.

Standards

  • ASTM: '904L'
  • UNS: N08904
  • EN Number: 1.4539
  • EN Name: X1NiCrMoCu25-20-5
  • W.Nr.: 1.4539
  • DIN: X 1 NiCrMoCu 25 20 5
  • SS: 2562
  • AFNOR: Z1NCDU25-20-4

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.