Sandvik 7C27Mo2 compressor valve steel

Strip steelDatasheet

Datasheet updated 2021-12-13 07:46 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 7C27Mo2 is a hardened and tempered martensitic stainless steel alloyed with molybdenum. The material is characterized by:

  • High strength
  • Very high fatigue strength under bending and impact stress
  • Excellent surface finish
  • High compressive residual surface stress
  • Low levels of non-metallic inclusions
  • Good wear resistance

Sandvik 7C27Mo2 compressor valve steel has good dimensional tolerances and good flatness.

Standards

  • UNS: S42026
  • EN Number: (1.4031)*

*) Nearest equivalent grade

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email