Sandvik Nanoflex®

Strip steelDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Nanoflex® is a precipitation hardening, austenitic stainless steel specifically designed for applications requiring high strength and good ductility. Mechanical strength can be increased substantially by heat treatment (ageing) of the final product, after first taking advantage of a soft 'as-delivered' condition, favorable for forming.

Normally, strip steel in Sandvik Nanoflex® is delivered in the cold rolled condition, but there is also a possibility of using the grade in the annealed condition and still reach a comparably high strength, solely by heat treatment.

Sandvik Nanoflex® is characterized by:

  • Very high tensile strength with comparably good ductility
  • Very high ageing effect
  • Hardenable by heat treatment from the annealed condition
  • No softening after exposure to temperatures up to 450°C (842°F)
  • Good weldability

Standards

  • ASTM: A693
  • UNS: S46910

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.