Sandvik Sanprint® EP

Strip steelDatasheet

Datasheet updated 2021-09-23 08:10 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Sanprint® EP is a hardened and tempered carbon steel used for printing doctor blade applications. The grade is a standard martensitic steel, particularly suitable for non water-based and UV inks and is characterized by:

  • Very high wear resistance
  • Good straightness
  • Excellent edge finish
  • Good dimensional tolerances

Standards

  • DIN: 100Cr6
  • SS: 2258

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email