Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 1C256 is a ferritic chromium steel for high-temperature applications. The grade is characterized by:

  • Good resistance to reducing sulphurous gases
  • Good resistance to oxidation in air

This steel can be used at temperatures up to 850°C (1560°F). However, allowance should be made for the low creep strength at the highest temperatures to avoid distortion due to the inherent mass of the steel.

Standards

  • EN Number: 1.4724**
  • W.Nr.: 1.4724*
  • DIN: X10CrAl13*

Product standards

  • SEW 470
  • EN 10095**

* Obsolete. Replaced by EN.
** Heat resisting steels and nickel alloys. Technical delivery conditions for sheet/plate, strip, bars, rods and sections.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.