Sandvik 316LVM for medical applications

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.

Sandvik 316LVM is a vacuum remelted, molybdenum alloyed, austenitic stainless steel.

The grade is characterized by:

  • High strength
  • High fatigue strength
  • Excellent microcleanliness
  • Excellent structural homogeneity
  • High surface finish

Standards

  • UNS: S31673
  • DIN: X 2 CrNiMo 18 15 3

Product standards

  • Bar and wire: ASTM F138

Disclaimer: Sandvik is not providing any products or services that are intended or may be construed to be recommending or otherwise advising on, in any manner, the design, suitability, appropriateness or effectiveness, from a medical/biological/safety perspective, of any medical material, instrument and/or medical device.