Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 3R60™ is an austenitic chromium-nickel steel with minimum 2.5% molybdenum and a low carbon content.

Sandvik 3R60™ is also available in a variant for the urea industry, Sandvik 3R60™ Urea Grade.

Standards

  • ASTM: TP316L, TP316
  • UNS: S31603, S31600
  • EN Number: 1.4435, 1.4436
  • EN Name: X 2 CrNiMo 18-14-3, X 3 CrNiMo 17-13-3
  • W.Nr.: 1.4435, 1.4436
  • DIN: X 2 CrNiMo 18 14 3, X 5 CrNiMo 17 13 3
  • SS: 2353, 2343
  • AFNOR: Z 2 CND 17.13
  • BS: 316S13
  • JIS: SU316LTP, 316TP, SU316LTB, 316TB

Product standards

  • ASTM A213, A269 and A312
  • JIS G3459
  • JIS G3463
  • EN 10216-5
  • BS 3605, 3606
  • DIN 17456, 17458
  • NFA 49-117*, 49-217*

* Mo content 2.00-2.40%

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.