Sandvik 5R75

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 07:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 5R75 is an austenitic, titanium-stabilized stainless chromium–nickel–molybdenum steel.

Standards

  • ASTM: TP316Ti
  • UNS: S31635
  • EN Number: 1.4571
  • EN Name: X6CrNiMoTi17-12-2
  • W.Nr.: 1.4571
  • DIN: X 6 CrNiMoTi 17 12 2
  • SS: 2350
  • AFNOR: Z6CNDT17-12

Product standards

Seamless tube and pipe:

  • ASTM A312
  • EN 10216-5
  • DIN 17456, 17458
  • SS 14 23 50
  • NFA 49-117
  • ASTM A213, A269 and A312

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.