Sandvik 8R41

Tube and pipe, seamlessDatasheet

Datasheet updated 2020-12-10 06:47 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 8R41 is a niobium-stabilized austenitic stainless steel.

Standards

  • EN Number: 1.4961
  • EN Name: X8CrNiNb16-13
  • W.Nr.: 1.4961
  • DIN: X 8 CrNiNb 16 13

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email