Sandvik Ti Grade 1 is an unalloyed titanium grade (CP titanium = commercially pure titanium) with low oxygen content. The grade is characterized by relatively low strength and high ductility. It is typically used for plate heat exchangers.
Standards
-
ASTM: Grade 1 -
UNS: R50250
Chemical composition (nominal)
Fe | O | C | H | N |
---|---|---|---|---|
≤0.20 | ≤0.12 | ≤0.08 | ≤0.01 | ≤0.02 |
Ti=Bal.