Sandvik Ti Grade 9

Tube and pipe, seamlessDatasheet

Datasheet updated 2021-06-10 17:10 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik Ti Grade 9 (Sandvik Ti 3Al-2.5V) is a titanium grade characterized by excellent corrosion resistance to seawater and higher mechanical properties than stainless steels. The Ti-3-2.5 alloy is characterized by:

  • Excellent resistance to general corrosion in seawater applications
  • High mechanical strength, superior strength to weight ratio
  • Resistant to stress corrosion cracking in chloride and sour gas environments
  • Excellent resistance to pitting, crevice, and erosion corrosion
  • Good formability and weldability
  • Very low thermal expansion
  • Excellent fatigue properties from Sandvik's proprietary processing that controls crystal texture

Standards

  • ASTM: Grade 9
  • UNS: R56320

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email