Sandvik 19.12.3.LR

Covered electrodes Datasheet

Datasheet updated 2018-10-23 14:30 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.12.3.LR (316/316L-17) is a chromium-nickel-molybdenum covered electrode with rutile coating for welding of low carbon, molybdenum alloyed, austenitic stainless steels of 316L (1.4436) type.

Standards

  • ISO 3581: 19 12 3 L R
  • AWS A5.4/ASME SFA-5.4: E316/316-17
  • W.Nr.: 1.4430

Product Approvals

  • CE
  • CWB

Contact your nearest sales office for details.

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.