Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.9.LR (308/308L-17) is a chromium-nickel covered electrode with rutile coating for welding of low carbon 18% Cr/10% Ni austenitic stainless steels.

The electrode has excellent arc stability, low spatter and fast burn off rate with minimal stub loss. It is also characterized by improved moisture resistance, self peeling slag, easy post weld finishing. Sandvik 19.9.LR (308/308L-17) gives smooth uniform beads and works in any standard weld position.

Standards

  • [ISO 3581] 19 9 L R
  • [AWS A5.4/ASME SFA-5.4] E308/308L-17

Product Approvals

  • CE

Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.