Sandvik 27.31.4.LCuR

Covered electrodes Datasheet

Datasheet updated 2018-06-13 16:05 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 27.31.4.LCuR-16 (383-16) is a covered electrode of AWS 383-16 type with rutile-basic coating and normal metal recovery for welding of high-alloy austenitic stainless steels of UNS S08028 (e.g. Sanicro 28) and Alloy 825 type (e.g. Sanicro 41).

Standards

  • ISO 3581: 27 31 4 Cu L R
  • AWS A5.4/ASME SFA-5.4: E(383)-16
  • W.Nr.: (1.4563)*

Product Approvals

TÜV

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

*nearest equivalent

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.