Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 60 is a nickel-chromium-molybdenum covered electrode for welding of Ni/Cr/Mo nickel alloys, high-alloy stainless steels and 5-9%Ni steels in cryogenic applications. It can used in many variants of dissimilar joining of nickel alloys, stainless steels and low alloyed steels. Sanicro® 60 can also be used for overlay welding on low alloyed steels.

The electrode combines good welding properties in all positions with very low impurity levels, high impact strength and excellent corrosion resistance to pitting in chloride containing media and stress corrosion cracking.

Standards

  • ISO 14172: Ni6625
  • AWS A5.11/ASME SFA-5.11: ENiCrMo-3
  • W.Nr.: 2.4621

Contact your nearest sales office for details.

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.