Sanicro® 71

Covered electrodes Datasheet

Datasheet updated 2018-07-05 13:53 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 71 is a covered electrode with basic coating and normal metal recovery for welding of NiCrFe alloys such as Alloy 600, 800, and 800H, 9% Ni steels as well as nickel-alloyed steels for cryogenic temperature use. It is also used for dissimilar joints, such as stainless steel and NiCu alloys to carbon steel and nickel alloys. Sanicro® 71 is characterized by little spatter and very good slag removal.

Standards

  • ISO: 14172: Ni6182
  • AWS A5.11/ASME SFA-5.11: ENiCrFe-3
  • W.Nr.: 2.4807

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.