AquaSan Ni50

Covered electrodesDatasheet

Datasheet updated2018-05-17 15:59 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

AquaSan Ni50 is a specially formulated, nickel based covered electrode with a waterproof coating for the welding of high strength steels with a Carbon Equivalent (CE) >0.4.

AquaSan Ni50 is specified for welding base materials with a CE >0.4, which are susceptible to hydrogen embrittlement. Nickel has a high affinity for hydrogen and this composition allows hydrogen to diffuse into the weld metal and away from the high strength steel.

Standards

  • AWS A5.35: (pending initial publication).

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.