Sandvik 19.13.4.L T1

Flux cored wire electrodes Datasheet

Datasheet updated 2017-01-19 12:29 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.13.4.L–T1 (317/317L-T1) is a chromium-nickel-molybdenum flux core electrode for welding of low carbon 18% Cr/10% Ni/ 3%Mo austenitic stainless steels of type 317.

The electrode has excellent arc stability, low spatter and fast burn off rate. It is also characterized by improved moisture resistance, self-peeling slag and easy post weld finishing. Sandvik 19.13.4.L–T1 (317/317L-T1) gives smooth uniform beads and works in any standard weld position.

Standards

  • AWS A5.22/ASME A5.22: E317-T1-1/T1-4
  • W.Nr.: 1.4438

Product Approvals

  • AWS

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email