Sandvik 19.12.3.L

Welding strip Datasheet

Datasheet updated 2018-05-24 15:42 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.12.3.L is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 19%Cr/12%Ni/3%Mo composition on carbon- and low alloyed steels.

The buffer layer is deposited using an over-alloyed consumable, such as Sandvik 21.13.3.L, Sandvik 22.11.L or Sandvik 24.13.L.

Standards

  • ISO 14343: 19 12 3 L
  • AWS A5.9/ASME SFA 5.9: EQ316L

Product Approvals

  • Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.