Sandvik 19.9.LNb

Welding strip Datasheet

Datasheet updated 2017-03-23 16:45 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.9.LNb is a niobium stabilized chromium-nickel strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of stabilized 19%Cr/9%Ni composition on carbon- and low alloyed steels.

The buffer layer is deposited using an over-alloyed consumable, such as Sandvik 21.11.LNb or Sandvik 24.13.LNb.

Standards

  • ISO 14343: 19 9 Nb
  • AWS A5.9/ASME SFA5.9: EQ347

Product Approvals

Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.