Sandvik 23.11.LNb

Welding strip Datasheet

Datasheet updated 2017-03-23 16:56 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 23.11.LNb is a niobium stabilized chromium-nickel strip electrode particularly suited for high speed electro-slag welding (ESW) to deposit a single layer overlay of stabilized corrosion resistant alloy of 19%Cr/9%Ni composition on carbon- and low alloyed steels. It can also be combined with Sandvik 19.9.LNb for surfacing of two layer overlays.

Standards

  • ISO 14343: 23 12 L Nb
  • AWS A5.9/ASME SFA5.9: EQ”309LNb”

Product Approvals

Contact your nearest sales office for details,

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.