Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 24.13.LNb is a niobium stabilized chromium-nickel strip electrode used for submerged arc welding (SAW) to deposit a buffer layer of stabilized corrosion resistant alloy of 19%Cr/9%Ni composition on carbon- and low alloyed steels. In high speed electro-slag welding (ESW) it can be used for single layer deposits of 347 composition on carbon- and low alloyed steels. It can also be combined with Sandvik 19.9.LNb for surfacing of two layer overlays.

Standards

  • ISO 14343: 23 12 Nb
  • AWS A5.9/ASME SFA5.9: EQ”309LNb”

Product Approvals

Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.