Sandvik 25.22.2.LMn

Welding strip Datasheet

Datasheet updated 2017-03-23 16:58 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 25.22.2.LMn is a chromium-nickel-molybdenum strip electrode used for electro-slag welding (ESW) or submerged arc welding (SAW) to deposit a second layer corrosion resistant alloy of 25%Cr/22%Ni/2%Mo composition on carbon- and low alloyed steels. It can also be used as buffer layer before depositing second layers.

Standards

  • ISO 14343: 25 22 2 N L
  • AWS A5.9/ASME SFA5.9: EQ”310LMo”

Product Approvals

Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.