Sanicro® 60

Welding strip Datasheet

Datasheet updated 2018-07-05 13:55 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 60 is a nickel-chromium-molybdenum strip electrode used for electro-slag welding (ESW) to deposit a second layer corrosion resistant alloy of Ni6625/UNS N06625 composition on carbon- and low alloyed steels.

It can also be used as buffer layer before depositing second layers. Due to the low carbon content of the strip Sanicro® 60 is often used for single layer deposits when the required Fe content in the overlay is less than 10%.

The grade is characterized by:

  • Excellent resistance to stress corrosion cracking in chlorides
  • Very good resistance to pitting and intergranular corrosion

Standards

  • ISO 18274: NiCr22Mo9Nb/Ni 6625
  • AWS A5.14/ASME SFA 5.14: EQNiCrMo-3

Product Approvals

Contact your nearest sales office for details.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.