Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sanicro® 69HP is a strip electrode used mainly in the nuclear industry to obtain a ENiCrFe-7 (UNS N06690) corrosion resistant overlay weld deposit on carbon, carbon-manganese and low-alloy steels using electroslag welding (ESW) with Sandvik 59S flux. Other combinations and conditions are possible.

Standards

  • ISO: Ni6043
  • AWS A5.14/ASME SFA5.14: EQNiCrFe-14

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.