Sandvik 13.4

Welding wire Datasheet

Datasheet updated 2018-07-24 14:27 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 13.4 is a filler material for the welding of parent metals of similar composition. The weld metal has high hardness and erosion resistance.

Standards

  • ISO 14343: 13 4
  • AWS A5.9/ASME SFA-5.9: ER410NiMo
  • W.Nr.: 1.4351

Please note that the Werkstoff Nr. corresponds to the base material of the same grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.