Sandvik 18.LNb

Welding wire Datasheet

Datasheet updated 2018-06-01 09:42 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 18.LNb is a filler material suitable for joining Cr-steels with max 18% Cr, stabilized or non-stabilized. It is available as wire and rods for MIG/MAG, TIG and plasma-arc welding.

Standards

  • ISO 14343: 18 L Nb
  • W.Nr.: 1.4511

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.