Sandvik 19.12.3.LSi

Welding wire Datasheet

Datasheet updated 2019-07-12 13:55 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.12.3.LSi is suitable for joining stainless Cr-Ni-Mo and Cr-Ni steels, stabilized or non-stabilized, e.g. ASTM 316, 316L and 316Ti as well as 304, 304L, 321 and 347,

Standards

  • ISO 14343: 19 12 3 L Si
  • AWS A5.9/ASME SFA-5.9: ER316LSi
  • W.Nr.: 1.4430

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.