Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.12.3.NbSi is suitable for joining chromium-nickel-molybdenum steels, stabilized or non-stabilized, e.g. ASTM 316Ti, 316 and 316L.

Standards

  • ISO 14343A: 19 12 3 Nb Si
  • AWS A5.9/ASME SFA-5.9: ER”318Si”
  • W.Nr.: 1.4576

Product Approvals

  • TÜV
  • UDT

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.