Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 19.13.4.L is suitable for joining stainless CrNiMo steels e.g. 317L or similar.

Standards

  • ISO 14343A: 19 13 4 L
  • AWS A5.9/ASME SFA-5.9: ER317L
  • W.Nr.: (1.4438)*

* nearest equivalent

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.