Sandvik 22.12.HT

Welding wire Datasheet

Datasheet updated 2017-09-19 16:31 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 22.12.HT is an austenitic filler material for welding the high temperature steel grade Sandvik 253 MA*, UNS S30815. It is characterized by high creep strength, good resistance to oxidation and good weldability.

Standards

  • W.Nr.: 1.4829

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.