Sandvik 22.8.3.L

Welding wire Datasheet

Datasheet updated 2019-07-12 14:38 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 22.8.3.L is a duplex stainless filler metal for welding duplex stainless steels. Weldability as well as properties of the all-weld metal is excellent. Corrosion resistance is equal to 904L in most applications.

Standards

  • ISO 14343: 22 9 3 N L
  • AWS A5.9/ASME SFA-5.9: ER2209
  • W.Nr.: 1.4462

Product Approvals

  • CE
  • DNV
  • TÜV

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.