Sandvik 23.7.L

Welding wire Datasheet

Datasheet updated 2017-09-19 15:36 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 23.7.L is a duplex stainless filler metal for welding lean duplex stainless steels such as Sandvik SAF 2304, LDX 2101* and similar. Corrosion resistance is equal to 316L in most applications. This alloy is not alloyed with molybdenum and has found applications for production of Nitric Acid in the fertilizer industry.

Standards

  • ISO 14343: 23 7 L N

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.