Sandvik 24.13.L

Welding wire Datasheet

Datasheet updated 2017-09-19 15:36 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 24.13.L is suitable for joining stainless Cr-Ni steels of the 309 type, Cr-steels and dissimilar steels.

Standards

  • ISO 14343: 23 12 L
  • AWS A5.9/ASME SFA-5.9: ER309L
  • W.Nr.: 1.4332

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.