Sandvik 24.13.LNb

Welding wire Datasheet

Datasheet updated 2017-09-19 16:21 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 24.13.LNb is a niobium-stabilized filler metal for overlay welding of carbon and low-alloy steels, where a type 347 of overlay is required.

Standards

  • ISO 14343: 23 12 Nb
  • AWS A5.9/ASME SFA-5.9: ER”309LNb”
  • W.Nr.: 1.4332

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Send PDF via email