Sandvik 24.16.3.L

Welding wire Datasheet

Datasheet updated 2018-07-23 11:55 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 24.16.3.L is a filler material for overlay welding on carbon and low-alloy steels where a 316L weld deposit is specified.

Standards

  • ISO 14343: (23 12 2 L)
  • AWS A5.9/ASME SFA-5.9: ER(309LMo)
  • W.Nr.: 1.4459

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.