Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 25.10.4.L welding wire has been specially developed for welding Sandvik SAF 2507 and other super-duplex steels.

Standards

  • [ISO 14343] 25 9 4 N L
  • [AWS A5.9/ASME SFA-5.9] ER2594
  • (1.4410)*

Product Approvals

  • CE
  • DNV
  • TÜV

* nearest equivalent

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.