Sandvik 25.20.C

Welding wire Datasheet

Datasheet updated 2017-09-19 16:23 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 25.20.C is a filler material for joining heat resistant austenitic steels of the 25 Cr/20 Ni type.

Standards

  • ISO 14343: 25 20
  • AWS A5.9/ASME SFA5.9: ER310
  • W.Nr.: 1.4842

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.