Sandvik 25.20.L

Welding wire Datasheet

Datasheet updated 2017-09-19 16:24 (supersedes all previous editions)

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.

Sandvik 25.20.L is a filler wire for joining Sandvik 2RE10 (UNS S31002) and similar grades used in heavily oxidizing media such as pipes in preheaters, coolers and condensers in the chemical industry. Sandvik 25.20.L can used for gas-shielded arc and gas-tungsten arc welding.

Standards

  • AWS A5.9/ASME SFA-5.9: ER"310L"
  • W.Nr.: 1.4842

Please note that the Werkstoff Nr. corresponds to the base material of the grade.

Disclaimer: Recommendations are for guidance only, and the suitability of a material for a specific application can be confirmed only when we know the actual service conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Sandvik materials.